| Performance |
Unit |
Typical value |
Test method |
| 3425-R15 |
3425-LR2-P4 |
| Tensile strength |
MPa |
12.4 |
12.8 |
GB/T 1040.3
|
| Elongation at break |
% |
290 |
195 |
| Thermal aging (158°C × 168 h) |
|
|
|
|
| Rate of change in tensile strength |
% |
+8 |
+11 |
GB/T 2951.12
|
| Rate of change of elongation at break |
% |
-10 |
-13 |
| Impact Brittleness Performance |
°C |
-40 |
-40 |
GB/T 5470
|
| Hot Extension Test (200°C) |
|
|
|
|
| Elongation under load |
% |
30 |
30 |
GB/T 2951.21
|
| Permanent deformation |
% |
5 |
5 |
| Volume resistivity at 20°C |
Ω.m |
7.0×10 13 |
5.0×10 12 |
GB/T 1410
|
| Dielectric strength |
MV/m |
25 |
25 |
GB/T 1408.1
|
| Electrical conductivity |
μS/mm |
1.2 |
1.2 |
GB/T17650.2
|
| pH value |
- |
5.5 |
5.5 |
| Halogen acid gas release amount |
mg/g |
1 |
1 |
GB/T 17650.1
|
| Maximum Smoke Density (Flaming) |
- |
55 |
50 |
GB/T 8323
|
| Maximum Smoke Density (Flameless) |
- |
252 |
260 |
| Oxygen Index |
- |
/ |
32 |
GB/T 2406.2
|