| Performance |
Unit |
Typical value |
| 3501 |
3521 |
3521-B |
3531 |
| Tensile strength |
MPa |
12 |
12.3 |
11.9 |
9 |
| Elongation at break |
% |
160 |
183 |
171 |
128 |
| Thermal aging |
|
|
|
|
|
| Test temperature |
°C |
100 |
110 |
110 |
- |
| Test duration |
h |
168 |
240 |
240 |
- |
| Rate of change in tensile strength |
% |
10 |
15 |
19 |
- |
| Rate of change of elongation at break |
% |
-9 |
-9 |
-11 |
- |
| Thermal stress cracking (130°C × 1 h) |
|
No cracks |
No cracks |
No cracks |
- |
| Hot-water immersion test (70°C × 168 h) |
|
|
|
|
|
| Rate of change in tensile strength |
% |
- |
-21 |
-25 |
- |
| Rate of change of elongation at break |
% |
- |
-18 |
-23 |
- |
| Low-temperature impact embrittlement performance |
°C |
-40 |
-40 |
-40 |
- |
| Volume resistivity at 20°C |
Ω.m |
9×10 12 |
5×10 11 |
2×10 11 |
- |
| Dielectric strength |
MV/m |
24 |
26 |
24 |
26 |
| Electrical conductivity |
μS/mm |
1.4 |
1.2 |
1.4 |
1.1 |
| pH value |
- |
5.2 |
5.2 |
5.2 |
5.7 |
| Halogen acid gas release amount |
mg/g |
<1 |
<1 |
<1 |
<1 |
| Maximum Smoke Density (Flaming) |
- |
66 |
58 |
50 |
44 |
| Maximum Smoke Density (Flameless) |
- |
256 |
243 |
225 |
197 |
| Oxygen Index |
- |
30 |
32 |
35 |
46 |