| Project |
Unit |
Standard value |
Typical value |
Test method |
| 3521-A |
3521-AH |
| Tensile strength |
MPa |
≥10 |
11.5 |
12.8 |
GB/T 1040 |
| Elongation at break |
% |
≥160 |
178 |
173 |
| Thermal aging (110±2℃ × 240 h) |
|
|
|
|
GB/T 1040 |
| Rate of change in tensile strength |
% |
±25 |
18 |
22 |
GB/T 2951.2 |
| Rate of change of elongation at break |
% |
±25 |
-13 |
-9 |
| Hot deformation (90°C) |
% |
≤50 |
18 |
22 |
GB/T8815 |
| Impact embrittlement temperature: -25°C |
- |
≤15/30 |
0/30 |
0/30 |
GB/T 5470 |
| Halogen acid gas release amount |
mg/g |
≤5 |
1 |
1 |
GB/T17650.1 |
| pH value |
|
≥4.3 |
5.9 |
5.7 |
GB/T 17650.2 |
| Electrical conductivity |
μS/mm |
≤10 |
1.2 |
1.1 |
GB/T 17650.2 |
| Maximum Smoke Density (Flaming) |
Dm |
≤100 |
60 |
48 |
GB/T 8323.2 |
| Maximum Smoke Density (Flameless) |
Dm |
≤350 |
190 |
189 |
B/T 8323.2 |
| Oxygen Index |
OI% |
≥36 |
37 |
40 |
GB/T 2406 |
| Volume resistivity at 20°C |
Ω.m |
≥1.0×10 10 |
3.5×10 12 |
8.0×10 11 |
GB/T1410 |
| Dielectric strength |
MV/m |
≥20 |
29 |
29 |
GB/T1408.1 |